If it's possible add induction treatment on the pin of forged chain?
A
pin of drop forged chain

Generally, the hardness of the pin of drop fogrged chain,like X348,X458,X678  is 40-44HRC.

If making induction treatment , the hardness can reach HRC58-62, the chain will be more wearable.